Inconel Alloy X750 N07750 2.4669 Superalloy Strip Nickel Alloy Strip

    Buy cheap Inconel Alloy X750 N07750 2.4669 Superalloy Strip Nickel Alloy Strip from wholesalers
     
    Buy cheap Inconel Alloy X750 N07750 2.4669 Superalloy Strip Nickel Alloy Strip from wholesalers
    • Buy cheap Inconel Alloy X750 N07750 2.4669 Superalloy Strip Nickel Alloy Strip from wholesalers
    • Buy cheap Inconel Alloy X750 N07750 2.4669 Superalloy Strip Nickel Alloy Strip from wholesalers
    • Buy cheap Inconel Alloy X750 N07750 2.4669 Superalloy Strip Nickel Alloy Strip from wholesalers
    • Buy cheap Inconel Alloy X750 N07750 2.4669 Superalloy Strip Nickel Alloy Strip from wholesalers
    • Buy cheap Inconel Alloy X750 N07750 2.4669 Superalloy Strip Nickel Alloy Strip from wholesalers
    • Buy cheap Inconel Alloy X750 N07750 2.4669 Superalloy Strip Nickel Alloy Strip from wholesalers

    Inconel Alloy X750 N07750 2.4669 Superalloy Strip Nickel Alloy Strip

    Ask Lasest Price
    Brand Name : FUSHUN
    Model Number : X750
    Certification : ISO 9001
    Payment Terms : TT LC DP
    Supply Ability : 3000 TONS PER YEAR
    Delivery Time : 20 DAYS
    • Product Details
    • Company Profile

    Inconel Alloy X750 N07750 2.4669 Superalloy Strip Nickel Alloy Strip

    Inconel Alloy X750, N07750, 2.4669 Superalloy


    Strip

    Delivery condition: cold-rolled, heat-treated and pickled or bright-annealed

    Thickness mm (in): 0,025-3 (0.001-0.12)

    Width mm (in): 4-750 (0.16-29.5)

    Rolled sheet – separated from the coil – are available in lengths from 250 - 4,000 mm (9.84-157.48 in).


    Introduce

    Fushun Metal is your high quality manufacturer of Nickel, Nickel-based, Copper-Nickel, Iron-Nickel Wire, Bar, Plate, Strip, Pipe and Forged products. We melt alloys in our EAF/VIM/VAR/LF/VOD furnaces and subsequent ESR refining processes can be employed for the most critical alloys. The ingots are then hot-worked by rolling or forging, followed by mechanical finishing such as peeling, turning, or cold working on one of our draw benches. According to customer request, we can employ special heat treatment procedures, drawing, straightening and sawing to length to achieve particular dimensions and tolerances. You also have the opportunity to specify both standard as well as modified chemical analyses.


    INCONEL alloy X-750 (UNS N07750/W. Nr. 2.4669) is a precipitation-hardenable nickel-chromium alloy used for its corrosion and oxidation resistance and high strength at temperatures to 1300°F. Although much of the effect of precipitation hardening is lost with increasing temperature over 1300°F, heat-treated material has useful strength up to 1800°F. Alloy X-750 also has excellent properties down to cryogenic temperatures.


    Application

    Inconel X-750 is used to fabricate flat springs and sheet metal stampings that are used in very high temperature applications such as jet engine parts, nuclear power plant

    applications, heat-treating fixtures, forming tools, and extrusion dies.

    •Gas turbine rotor blades, wheels and bolts

    •Airframe thrust reversers and hot-air ducting systems

    •Rocket engine thrust chambers

    •Heat treat fixtures and cryogenic vessels, springs and fasteners


    Standard and Grade

    INCONEL alloy X-750 is designated as UNS N07750 and W. Nr. 2.4669. The alloy is stated in NACE MR-01-75. Available product forms are sheet, strip, plate, round bar, flat bar, forging stock, hexagon, wire, tubing and extruded section. Specifications include the following:

    •Rod, Bar and Forging - ASTM/ASME SB637; ISO 9723-9725; SAE AMS 5667-5671 5747; EN 10269

    •Plate, Sheet and Strip - ISO 6208, SAE AMS 5542 and 5598.

    •Wire - BS HR 505, SAE AMS 5698 and 5699.


    Chemical Component

    X-750Ni(+Co)CrFeTiAlNo(+Ta)SiSCuCCo
    Min701452.250.40.7-----------
    Max--1792.7511.20.50.010.50.081

    Mechanical Properties

    INCONEL alloy X-750 may be given any one of a variety of heat treatments. Each develops special properties and puts the product form in the best condition for its intended application. In all conditions, alloy X-750 is resistant to oxidation up to 1800°F. The most often used heat treatments have been incorporated by the Society of Automotive Engineers in their AMS specifications* for various product forms.

    Density

    0.299 lb/inᶟ

    8.28 g/cmᶟ

    Melting Range

    2540-2600°F

    1395-1425°C

    Curie Temperature °F

    *as hot-rolled -225

    *triple-heat-treated (2100°F/2 hr, A.C., +1500°F/24 hr, A.C. + 1300°F/20 hr, A.C.) -193

    Magnetic Permeability 70°F, 200H

    *as hot rolled - 1.0020

    *triple-heat-treated (2100°F/2 hr, A.C., +1500°F/24 hr, A.C.,+1300°F/20 hr, A.C.) - 1.0035

    Emissivity Oxidized Surface

    600°F - 0.895

    2000°F - 0.925

    Linear Contraction During Precipitation Treatment (1300°F/20 hr), in/in

    Hot-rolled - 0.00044

    20% Cold-rolled - 0.00052

    Annealed - 0.00026


    Inspection

    In order to ensure consistently high levels of material and processing properties, we have our own fully equipped laboratory. We closely monitor your order throughout the production process right from the raw material, via the interim stages to the finished product. We employ the very latest technology for chemical analysis, metallography and mechanical testing. With the help of our expert partners, we can also offer non-standard testing methods.


    Package & Logistics

    all of our steel products are packaged as per international standard to prevent any possible damage or loss. For enhanced customer experience, we also provide dedicated package as per your special requirements.

    By default, we will quote based on sea transportation, such as FOB, CFR, CIF, DDU, DDP and the like for most enquiries or orders. Quotation based on air transportation is also optional upon your request for urgent demands.


    Quality Inconel Alloy X750 N07750 2.4669 Superalloy Strip Nickel Alloy Strip for sale
    • Haven't found right suppliers
    • Our buyer assistants can help you find the most suitable, 100% reliable suppliers from China.
    • And this service is free of charge.
    • we have buyer assistants who speak English, French, Spanish......and we are ready to help you anytime!
    Submit Buying Request
    Send your message to this supplier
    *From:
    Your email address is incorrect!
    *Subject:
    Your subject must be between 10-255 characters!
    *Message:
    For the best results, we recommend including the following details:
    • --Self introduction
    • --Required specifications
    • --Inquire about price/MOQ
    Your message must be between 20-3,000
    Yes! I would like your verified suppliers matching service!
    Send your message to this supplier
     
    *From:
    *To: Hunan Fushun Metal Co., Ltd.
    *Subject:
    *Message:
    Characters Remaining: (0/3000)
     
    Explore more Others products from this supplier
    Find Similar Products By Category:
    Ore
    Inquiry Cart 0