Sign In | Join Free | My burrillandco.com
Home > Nickel >

UNSR30605 UNS Light Rod Plate High Temp Alloys Ni Based Superalloys

    Buy cheap UNSR30605 UNS Light Rod Plate High Temp Alloys Ni Based Superalloys from wholesalers
     
    Buy cheap UNSR30605 UNS Light Rod Plate High Temp Alloys Ni Based Superalloys from wholesalers
    • Buy cheap UNSR30605 UNS Light Rod Plate High Temp Alloys Ni Based Superalloys from wholesalers
    • Buy cheap UNSR30605 UNS Light Rod Plate High Temp Alloys Ni Based Superalloys from wholesalers
    • Buy cheap UNSR30605 UNS Light Rod Plate High Temp Alloys Ni Based Superalloys from wholesalers
    • Buy cheap UNSR30605 UNS Light Rod Plate High Temp Alloys Ni Based Superalloys from wholesalers
    • Buy cheap UNSR30605 UNS Light Rod Plate High Temp Alloys Ni Based Superalloys from wholesalers
    • Buy cheap UNSR30605 UNS Light Rod Plate High Temp Alloys Ni Based Superalloys from wholesalers
    • Buy cheap UNSR30605 UNS Light Rod Plate High Temp Alloys Ni Based Superalloys from wholesalers

    UNSR30605 UNS Light Rod Plate High Temp Alloys Ni Based Superalloys

    Ask Lasest Price
    Brand Name : KAIXIN
    Model Number : KX-Alloy605
    Certification : ISO9001:2015
    Price : To negotiate
    Payment Terms : T/T, L/C
    Supply Ability : 50~80TONS per MONTH
    Delivery Time : 45~60days
    • Product Details
    • Company Profile

    UNSR30605 UNS Light Rod Plate High Temp Alloys Ni Based Superalloys

    KX UNSR30605 Uns Light Rod Plate Structural Operating Temperature Range For High Temperature Alloy


    Product Description and Application

    UNSR30605 is also known as L605,GH5605,GH605

    UNSR30605 is a Co-Cr-Ni based solid solution enhanced deformation superalloy, its use temperature is below 1000℃. Cobalt-based superalloy UNSR30605 is a cobalt base alloy strengthened by solution of 20%Cr and 15%W(percent mass). It has medium durability and creep strength below 815℃, excellent oxidation resistance below 1 090℃, and satisfactory process properties such as forming and welding. It is a key material for aero engine, rocket engine, naval ship and industrial gas turbine. Its development and production status is one of the symbols on the metal materials development level in a country. It is used for manufacturing the high temperature parts of aero engine guide blade, turbine outer ring, outer wall, swirler and sealing plate.


    Process Performance and Requirements


    • Product Fusion Process

    Vacuum Induction Furnace(VIM) and Electroslag Remelting Furnace(ESR)


    • Product Chemical Composition

    CompositionFeCSiMnPSCrNiWMore
    Min-0.05-1--19914Co:Rem
    Max30.150.420.040.03211116

    • Product Physical Property

    Densityp=9.13g/cm3
    Melting Temperature Range1330℃-1410℃

    • Product Mechanical Property

    VarietyTensile Property in the Room Temperature

    Hardness

    HV

    815℃ DurabilityGrain Size/GradeOther properties
    MPaMPaMPaMPat/h%
    Middle Plate,Sheet,Strip≧890370-550≧35≤290165≧24≧10≧2.5(1)Bend

    Cold Hard Strip

    Grade A

    ≧1500≧1300≧5410-480----------≧9Bend

    Cold Hard Strip

    Grade B

    ≧1700≧1500≧3485-560---------≧10Bend
    Bar≧860≧340≧35≤ 282165≧ 23≧10≧2(0)---
    Ring≧860≧310≧30≤ 248165≧ 24≧10≧2(0)---

    • Productive Process


    • Professional Customization

    Cold-drawn Wire¢0.3~¢18mm(Delivery in rolls or trays)
    Hot-Rolling Wire¢5.5~¢20mm(Delivery in rolls)
    Stripthickness 0.1~4.5*width 6~350mm(Supply in rolls or straight strips)
    Smooth Forged Rod on a Lathe

    ¢60~350mm,L800-2500mm

    Hot-rolled Burnishing¢20~80mm,L1000-5000mm
    Cold Drawn and Burnishing¢2.5~18mm,L1000-8000mm
    Seamless Tube¢1~275mm,wall thickness 0.2~30,L1000-8000mm

    Quality UNSR30605 UNS Light Rod Plate High Temp Alloys Ni Based Superalloys for sale
    • Haven't found right suppliers
    • Our buyer assistants can help you find the most suitable, 100% reliable suppliers from China.
    • And this service is free of charge.
    • we have buyer assistants who speak English, French, Spanish......and we are ready to help you anytime!
    Submit Buying Request
    Send your message to this supplier
    *From:
    Your email address is incorrect!
    *Subject:
    Your subject must be between 10-255 characters!
    *Message:
    For the best results, we recommend including the following details:
    • --Self introduction
    • --Required specifications
    • --Inquire about price/MOQ
    Your message must be between 20-3,000
    Yes! I would like your verified suppliers matching service!
    Send your message to this supplier
     
    *From:
    *To: Danyang Kaixin Alloy Material Co., Ltd.
    *Subject:
    *Message:
    Characters Remaining: (0/3000)
     
    Explore more High Temperature Alloy products from this supplier
    Find Similar Products By Category:
    Inquiry Cart 0