    OEM Hot Runner Typical Injection Molding Defects Analysis And Solutions

    Ask Lasest Price
    Price : Negotiable
    Payment Terms : T/T
    Supply Ability : More than 1 million
    Delivery Time : 30day
    Brand Name : OEM
    Certification : ISO
    • Product Details
    • Company Profile

    OEM Hot Runner Typical Injection Molding Defects Analysis And Solutions

    The Cause And Countermeasure Of Product Leaving Marks

    Current Ripple


    When the material in the mold is solidified and the molten material after the flow is mixed, such as Mi is not fully integrated, there will be dim and scaly in the product. Iridescent or ring shaped, this phenomenon is the flow mark, usually occurs at a slow speed


    CauseCuntermeasure
    Forming condition

    1. The material overflow degree is too low, and the front section is very easy to cure

    2. Mold temperature is too low

    3. The speed of chaos molding is too fast or too slow, which will produce ripple flow marks when it is too slow and jagged flow marks when it is too fast

    4. The filling pressure or holding pressure is too low, so that the flow mark is clear

    show

    1. Increase the molding temperature

    2. Increase die temperature

    3. Set the right speed

    4. Increase filling and retaining pressure


    Die

    1. The gate is too small

    2. No cold feed well

    3. Improper pouring U position


    1.F pour n

    2. Open more cold feed Wells.

    3. If pouring U is not fixed, the material will also touch the position of trapping mold hole wall

    Product Design

    1. Product structure design makes more right angles

    2. The product is broken and the thickness difference is too large

    1. Improve product shape and smooth molten material flow

    2. Change the design to make the thickness too smooth

    Material

    1. Poor liquidity of materials

    2. Too much filler


    1. Improve liquidity

    2. Switch to materials with fewer fillers

    OtherBlockage of suona on injection molding machine

    Clean the nozzle of the machine


    Quality OEM Hot Runner Typical Injection Molding Defects Analysis And Solutions for sale
    • Haven't found right suppliers
    • Our buyer assistants can help you find the most suitable, 100% reliable suppliers from China.
    • And this service is free of charge.
    • we have buyer assistants who speak English, French, Spanish......and we are ready to help you anytime!
    Submit Buying Request
    Send your message to this supplier
    *From:
    Your email address is incorrect!
    *Subject:
    Your subject must be between 10-255 characters!
    *Message:
    For the best results, we recommend including the following details:
    • --Self introduction
    • --Required specifications
    • --Inquire about price/MOQ
    Your message must be between 20-3,000
    Yes! I would like your verified suppliers matching service!
    Send your message to this supplier
     
    *From:
    *To: Sun On Plastic Moulding Limited
    *Subject:
    *Message:
    Characters Remaining: (0/3000)
     
    Explore more Injection Molding Solution products from this supplier
    Find Similar Products By Category:
    Inquiry Cart 0