| Sign In | Join Free | My burrillandco.com |
|
| Ask Lasest Price | |
| Brand Name : | New Era |
| Model Number : | ASTM A178 |
| Certification : | ISO9001,TS16949 |
| Price : | Negotiation |
| Payment Terms : | T/T |
| Supply Ability : | 3000 tons/month |
| Delivery Time : | 45 days |
ASTM A178 Electric Resistance Welded Carbon Steel and Carbon Manganese Steel Boiler and Superheater Tubes
Material: Carbon steel and carbon manganese steel
Production: Electric Resistance Welding
Size range: O.D.: 12.7-127mm W.T.:0.9-9.1mm L: according to customer
requirement
Applications: For Boilers, Superheaters, Heat-Exchangers, Condensers, Boiler flues, Superheater flues and Safe ends
Heat treatment:
After welding, all tubes are heat treated at a temperature of 1650℉
(900℃) or higher and followed by cooling in air or in the cooling
chamber of a controlled atmosphere furnace.
Cold-Drawn tubes are heat treated after the final cold-draw pass at
a temperature of 1200℉(650℃)or higher.
Chemical Properties
| Element | Grade A,Low-Cabon Steel | Grade C,Medium-Carbon Steel | Grade D, Carbon-Manganese Steel | |
| Carbon | 0.06-0.18 | 0.35 Max | 0.27Max | |
| Manganese | 0.27-0.63 | 0.80Max | 1.00-1.50 | |
| Phosphorus,Max | 0.035 | 0.035 | 0.030 | |
| Sulfur,Max | 0.035 | 0.035 | 0.015 | |
| Silicon | - | - | 0.10 min | |
| Mechanical Properties | Grade A | Grade C | Grade D | |
| Tensile Strength:min ksi(Mpa) | 47(325) | 60(415) | 70(485) | |
| Yield Point:min ksi(Mpa) | 26(180) | 37(255) | 40(275) | |
| Elongation | ≥35% | ≥30% | ≥30% | |


|