Inconel 718 plus UNS N07818 Precipitation Hardened Nickel-base Superalloy

    Buy cheap Inconel 718 plus UNS N07818 Precipitation Hardened Nickel-base Superalloy from wholesalers
     
    Buy cheap Inconel 718 plus UNS N07818 Precipitation Hardened Nickel-base Superalloy from wholesalers
    • Buy cheap Inconel 718 plus UNS N07818 Precipitation Hardened Nickel-base Superalloy from wholesalers
    • Buy cheap Inconel 718 plus UNS N07818 Precipitation Hardened Nickel-base Superalloy from wholesalers
    • Buy cheap Inconel 718 plus UNS N07818 Precipitation Hardened Nickel-base Superalloy from wholesalers
    • Buy cheap Inconel 718 plus UNS N07818 Precipitation Hardened Nickel-base Superalloy from wholesalers

    Inconel 718 plus UNS N07818 Precipitation Hardened Nickel-base Superalloy

    Ask Lasest Price
    Brand Name : XUNSHI
    Model Number : N07818
    Certification : ISO9001:2015
    Price : Negotiable
    Payment Terms : T/T
    Supply Ability : 5000kg per month
    Delivery Time : 45-60 days
    • Product Details
    • Company Profile

    Inconel 718 plus UNS N07818 Precipitation Hardened Nickel-base Superalloy


    Inconel 718Plus alloy (UNS N07818) is a precipitation hardened nickel-base material that exhibits high temperature tensile strength and stress rupture performance. This alloy is designed to have the high temperature capability and thermal stability of Waspaloy alloy while retaining the processing characteristics of 718 alloy. It is double vacuum melted (VIM/ESR/VAR). This VIM/VAR process ensures excellent microcleanliness and tight compositional control. Triple melting, with electroslag remelting between the VIM and VAR operations, minimizes the possibility of macrosegregation, increases microcleanliness, and is preferred for premium quality jet engine rotating component applications. Inconel 718Plus alloy has at least a 100°F (55°C) operating temperature advantage over 718 alloy. 718Plus alloy also has advantages over Waspaloy and other higher temperature capable, nickel-base alloys due to its higher strength, superior formability, better wear resistance, and a resistance to weld cracking. 718Plus alloy is a lower cost option than Waspaloy or Rene 41 alloy due to its lower intrinsic raw materials cost and improved hot workability which provides higher material yields, resulting in a lower cost finished part.


    Chemical composition

    ElementCMnSiPSCrNiMoNbTiAlCoWBCuPbBiSeFe
    Weight(%)0.01-0.050.35 max0.35 max0.004-0.0200.0025 max17.00-21.00Rem2.50-3.105.20-5.800.50-1.001.20-1.708.00-10.000.80-1.400.003-0.0080.30 max0.0005 max0.00003 max0.0003 max8.00-10.00

    Hardness

    HRC 25 - 35(solution heat treated depending on quench rate)

    HRC 42 - 48(fully aged condition)

    Tensile Strength, Ultimate 1480 MPa


    Application

    These products have been typically used for parts requiring high resistance to creep and stress rupture up to 1400°F(760°C) and oxidation resistance up to 1800°F(982°C), but usage is not limited to such applications.


    Available forms

    718Plus alloy is available in all product forms: ingot, billet, block, forged round bar, hot-rolled shapes and rectangles, bar, rod, wire, plate, sheet, strip, and castings.

    Quality Inconel 718 plus UNS N07818 Precipitation Hardened Nickel-base Superalloy for sale
    • Haven't found right suppliers
    • Our buyer assistants can help you find the most suitable, 100% reliable suppliers from China.
    • And this service is free of charge.
    • we have buyer assistants who speak English, French, Spanish......and we are ready to help you anytime!
    Submit Buying Request
    Send your message to this supplier
    *From:
    Your email address is incorrect!
    *Subject:
    Your subject must be between 10-255 characters!
    *Message:
    For the best results, we recommend including the following details:
    • --Self introduction
    • --Required specifications
    • --Inquire about price/MOQ
    Your message must be between 20-3,000
    Yes! I would like your verified suppliers matching service!
    Send your message to this supplier
     
    *From:
    *To: Suzhou Xunshi New Material Co., Ltd
    *Subject:
    *Message:
    Characters Remaining: (0/3000)
     
    Explore more Inconel Nickel Alloy products from this supplier
    Find Similar Products By Category:
    Inquiry Cart 0