Sign In | Join Free | My burrillandco.com
Home > Other General Mechanical Components >

965 Tensile Strength Inconel Nickel Alloy Inconel 718 Tube With Stress Corrosion Cracking Resistance

    Buy cheap 965 Tensile Strength Inconel Nickel Alloy Inconel 718 Tube With Stress Corrosion Cracking Resistance from wholesalers
     
    Buy cheap 965 Tensile Strength Inconel Nickel Alloy Inconel 718 Tube With Stress Corrosion Cracking Resistance from wholesalers
    • Buy cheap 965 Tensile Strength Inconel Nickel Alloy Inconel 718 Tube With Stress Corrosion Cracking Resistance from wholesalers

    965 Tensile Strength Inconel Nickel Alloy Inconel 718 Tube With Stress Corrosion Cracking Resistance

    Ask Lasest Price
    Brand Name : BLM-DX-1
    Price : FobShanghai usd 5.9-6.4/kg
    Payment Terms : Western Union, L/C, T/T
    Supply Ability : 300 Ton/Tons per Month
    Delivery Time : 25-30 days subject to the clients' requirement and quantity
    • Product Details
    • Company Profile

    965 Tensile Strength Inconel Nickel Alloy Inconel 718 Tube With Stress Corrosion Cracking Resistance

    Inconel 718

    Inconel 718 Chemical composition


    Alloy%NiCrFeMoNbCoCMnSiSCuAlTi
    718Min.5017balance2.84.750.20.7
    Max.55213.35.510.080.350.350.010.30.81.15

    Inconel 718 Physical properties


    Density8.2 g/cm³
    Melting point1260-1340 ℃

    Inconel 718 Alloy minimum mechanical properties in the roomtemperature


    AlloyTensile strength Rm N/mm²Yield strength R P0. 2N/mm²Elongation A 5 %

    Brinell hardness

    HB

    Solution treatment96555030≤363

    718 Characteristic as below:

    1.workability

    2.High tensile strength,endurance strength,creep strength and rupture strength at 700℃.

    3.High inoxidability at1000℃. 4.Steady mechanical performance in the low temperature.

    5.Good welding performance.


    Inconel 718 Metallurgical structure


    718alloy is Austenitic structure, precipitation hardening generate "γ" made it excellent mechanical performance. G rain boundary generate "δ" made it the best plasticity in the heat treatment.


    Inconel 718 Corrosion resistance


    718 alloy with extremely resistance to stress corrosion cracking and pitting ability in high temperature or low temperature environments, especially the inoxidability in the high temperature.


    Inconel 718 Application field:

    1 . The elevated temperature strength, excellent corrosion resistance and workability at 700℃ properties

    2 . made it use in a wide range of high requirement environments :Steam turbine ; Liquid-fuel rocket ; Cryogenic engineering

    3.Acid environment

    4.Nuclear engineering



    Quality 965 Tensile Strength Inconel Nickel Alloy Inconel 718 Tube With Stress Corrosion Cracking Resistance for sale
    • Haven't found right suppliers
    • Our buyer assistants can help you find the most suitable, 100% reliable suppliers from China.
    • And this service is free of charge.
    • we have buyer assistants who speak English, French, Spanish......and we are ready to help you anytime!
    Submit Buying Request
    Send your message to this supplier
    *From:
    Your email address is incorrect!
    *Subject:
    Your subject must be between 10-255 characters!
    *Message:
    For the best results, we recommend including the following details:
    • --Self introduction
    • --Required specifications
    • --Inquire about price/MOQ
    Your message must be between 20-3,000
    Yes! I would like your verified suppliers matching service!
    Send your message to this supplier
     
    *From:
    *To: BLOOM(suzhou) Materials Co.,Ltd
    *Subject:
    *Message:
    Characters Remaining: (0/3000)
     
    Explore more Other Materials products from this supplier
    Find Similar Products By Category:
    Inquiry Cart 0