Sign In | Join Free | My burrillandco.com
Home > Other Metals & Metal Products >

Dental Cobalt Based Superalloys Superior Mechanical Performance Castability

    Buy cheap Dental Cobalt Based Superalloys Superior Mechanical Performance Castability from wholesalers
     
    Buy cheap Dental Cobalt Based Superalloys Superior Mechanical Performance Castability from wholesalers
    • Buy cheap Dental Cobalt Based Superalloys Superior Mechanical Performance Castability from wholesalers
    • Buy cheap Dental Cobalt Based Superalloys Superior Mechanical Performance Castability from wholesalers

    Dental Cobalt Based Superalloys Superior Mechanical Performance Castability

    Ask Lasest Price
    Brand Name : Willett
    Model Number : 45CCF02
    Price : Contact for pricing
    Payment Terms : L/C, T/T, Western Union, MoneyGram
    Supply Ability : 50 + KG + per day
    Delivery Time : 5-8 Business days
    • Product Details
    • Company Profile

    Dental Cobalt Based Superalloys Superior Mechanical Performance Castability

    45% Cobalt Chrome Dental Casting Alloys for Frames


    Engraving service is available for Our Cobalt Chrome dental alloy. The letter "45CF" will be engraved on the body of each ingot of alloy. It will be helpful for Lab technician to differentiate different alloy in their lab. Our 45% cobalt chrome dental casting alloys contain less amount of Cobalt enables the metal have lower melting temp. and greater flexibility. It consist the same resistance to traction comapres to regular Cobalt Chrome alloy. They are perfect economical alternative to Gold & Silver based alloys (precious) without compromising its performance thanks to Willett's mechanical properties and biocompatibility.


    Advantages:


    (1). Superior mechanical performance castability, toughness.

    (2). Corrosion resistance, wear resistance, high intensity, great hardness.

    (3). Nickle-free guaranteed biocompatibility.

    (4). Much more economic than regular Cobalt Chrome alloy.


    Element Composition:


    CoCrOthers
    60%30%10%

    Properties:

    Melting Point1100-1200 Celsius
    Density8.5g/cm³
    Hardness380HV10

    FAQ:


    What is the perfect temperature to obtain the best result when casting?


    The casting temperature should always maintain 100~150℃ higher than liquidus temperature.


    What is the perfect timing to obtain the best result when casting?


    While casting Nickel Chrome alloys that don't contain Beryllium, the surface of the melting alloys will appear a layer of shadow. Once the shadow disappears and the edges of the alloy have become rounded (melted until it becomes a sphere shape is not necessary) will be the best timing for casting. Perfect timing for casting Cobalt Chrome alloy is to heat it till the surface membrane perforated and a spark of bright light start to appear.


    Cobalt Chrome casting piece is incomplete, what are the causes?


    1. Casting ring is not heated evenly: While casting Cobalt alloys, casting ring must heat up gradually and slowly before reaches 300℃. Let it sit in the oven in between 300℃ and 600℃ for 10-30 minutes. Once it heats up to the desired temperature, maintain the same temperature for at least 30 minutes before casting.


    2. Casting temperature is below/above alloy's requirement.


    3. Strub designed improperly: For example, Strub is too narrow. We strongly recommend the Strub diameter consist of 5mm or more.


    4. The amount of alloy is not enough for the casting piece or the centrifugal force of casting pressure is not enough.


    5. Casting piece has not avoided the heat center.


    Quality Dental Cobalt Based Superalloys Superior Mechanical Performance Castability for sale
    • Haven't found right suppliers
    • Our buyer assistants can help you find the most suitable, 100% reliable suppliers from China.
    • And this service is free of charge.
    • we have buyer assistants who speak English, French, Spanish......and we are ready to help you anytime!
    Submit Buying Request
    Send your message to this supplier
    *From:
    Your email address is incorrect!
    *Subject:
    Your subject must be between 10-255 characters!
    *Message:
    For the best results, we recommend including the following details:
    • --Self introduction
    • --Required specifications
    • --Inquire about price/MOQ
    Your message must be between 20-3,000
    Yes! I would like your verified suppliers matching service!
    Send your message to this supplier
     
    *From:
    *To: Success Dental Company
    *Subject:
    *Message:
    Characters Remaining: (0/3000)
     
    Explore more Cobalt Chrome Alloy products from this supplier
    Find Similar Products By Category:
    Inquiry Cart 0