GH132 Alloy Is A High-Strength Nickel-Based Superalloy With Excellent High-Temperature Stability And Oxidation Resistanc
GH132 Alloy is a high-performance nickel-based superalloy designed for demanding high-temperature applications. It is known for its exceptional strength and stability under elevated temperatures, making it ideal for use in aerospace and industrial environments.
Key Properties and Features:
GH132 Alloy’s superior performance in extreme conditions ensures it is a trusted choice for advanced engineering applications requiring high durability and reliability.
Here is a composition table for GH132 Alloy:
| Element | Composition Range (%) |
|---|---|
| Nickel (Ni) | 60.0 - 65.0 |
| Chromium (Cr) | 14.0 - 16.0 |
| Cobalt (Co) | 8.0 - 10.0 |
| Molybdenum (Mo) | 2.5 - 4.0 |
| Iron (Fe) | ≤ 6.0 |
| Titanium (Ti) | 1.0 - 2.0 |
| Aluminum (Al) | 1.0 - 2.0 |
| Carbon (C) | ≤ 0.10 |
| Manganese (Mn) | ≤ 0.5 |
| Silicon (Si) | ≤ 0.5 |
| Sulfur (S) | ≤ 0.01 |
These values are general guidelines. For specific applications or precise compositions, consult with industry standards or suppliers.

|