1060 3003 Heat Preservation Aluminum Coil Engineering Pipeline Anti-Corrosion Alloy Coil Spot Sales 1060 aluminum plate with 99.6% aluminum content, also known as pure aluminum plate, belongs to a commonly used...
...Coil For For Volkswagen /Audi A3 A4 A5 A6 RS4 TT VW Beetle Golf UF575 07K905715D 07K905715A Car Ignition Coil For For Volkswagen /Audi CAR MAKE FAW-Volkswagen - Magotan Audi Q5 Old Magotan 1.8TSI five-speed ...
...Coil Chemical Composition and Mechanical Property C Max Si Max Mn Max P Max S Max 0.23 0.6 1.8 0.040 0.040 Tensile Strength(MPa) Yield Strength(MPa) % Elongation in 2 in.(50mm) min Impacting Test Temperature...
...Coil Chemical Composition and Mechanical Property Grade Yield Strength (MPa) min. Tensile Strength (MPa) min. Elongation in 8 in. min. % Elongation in 2 in. min. % A656 Grade 80 550 620 12 15 Application A65...
...Coil Chemical Composition and Mechanical Property Grade Yield Strength (MPa) min. Tensile Strength (MPa) min. Elongation in 8 in. min. % Elongation in 2 in. min. % A656 Grade 70 485 550 14 17 Application A65...
...Coil Chemical Composition and Mechanical Property Grade Yield Strength (MPa) min. Tensile Strength (MPa) min. Elongation in 8 in. min. % Elongation in 2 in. min. % A656 Grade 60 415 485 17 20 Application A65...
...Coil Chemical Composition and Mechanical Property Grade Yield Strength (MPa) min. Tensile Strength (MPa) min. Elongation in 8 in. min. % Elongation in 2 in. min. % A656 Grade 50 345 415 20 23 Application A65...
...Coil Chemical Composition and Mechanical Property Grade Yield Strength (MPa) min. Tensile Strength (MPa) min. Elongation in 8 in. min. % Elongation in 2 in. min. % SA656 Grade 50 345 415 20 23 Application SA...
...) (t≤25.4mm) Elongation % min. (t≤25.4mm) 400 390 540 min. 16 Application SS540 carbon steel coil is used in the Construction of Bridges, Highway Construction and Other Engineering construction. Our...
...) (t≤25.4mm) Elongation % min. (t≤25.4mm) 285 275 490-610 19 Application SS490 carbon steel coil is used in the Construction of Bridges, Highway Construction and Other Engineering construction. Our...
...) (t≤25.4mm) Elongation % min. (t≤25.4mm) 245 235 400-510 21 Application SS400 carbon steel coil is used in the Construction of Bridges, Highway Construction and Other Engineering construction. Our...
...) (t≤25.4mm) Elongation % min. (t≤25.4mm) 205 195 330-430 26 Application SS330 carbon steel coil is used in the Construction of Bridges, Highway Construction and Other Engineering construction. Our...
...Coil Chemical Composition and Mechanical Property C Si Mn P S B Mo 0.10-0.20 0.15-0.30 1.10-1.50 0.035 0.035 0.001-0.005 0.45-0.55 Thickness (mm) Yield strength (≥Mpa) Tensile strength (Mpa) Elongation in ≥,...
...Coil Chemical Composition and Mechanical Property C max Si max Mn max P max S max Cu 0.23 0.40 1.35 0.04 0.05 1 Grade Yield Strength (MPa) min. Tensile Strength (MPa) min. Elongation in 8 in. min. % Elongati...
...Coil Chemical Composition and Mechanical Property C max Si max Mn P max S max Cu min 0.25 0.40 - 0.04 0.05 0.20 Grade Yield Strength (MPa) min. Tensile Strength (MPa) min. Elongation in 8 in. min. % Elongati...
... Strength (MPa) Elongation % min. 275 265 410-540 22 Application GB/T700 Q275A carbon steel coil is used in the Construction of Bridges, Highway Construction and Other Engineering construction. Our...
... Strength (MPa) Elongation % min. 235 225 370-500 26 Application GB/T700 Q235D carbon steel coil is used in the Construction of Bridges, Highway Construction and Other Engineering construction. Our...
... Strength (MPa) Elongation % min. 235 225 370-500 26 Application GB/T700 Q235C carbon steel coil is used in the Construction of Bridges, Highway Construction and Other Engineering construction. Our...
... Strength (MPa) Elongation % min. 235 225 370-500 26 Application GB/T700 Q235B carbon steel coil is used in the Construction of Bridges, Highway Construction and Other Engineering construction. Our...
...Coil Chemical Composition and Mechanical Property C max Si Mn P max S max 0.22 0.35 1.40 0.045 0.050 Yield Strength (MPa) min. (t≤16mm) Yield Strength (MPa) min.(16mm