...Molds Introduction of silicone putty MC- Silicone PUTTY are new silicone compounds (platinum catalyst) that can be easily mixed and applied by hand to a variety of surfaces. Silicone Putty is mixed in equal ...
...Curing Agent CA-30 Mixing ratio 100:2 Mixed Viscosity 10000cps Working time 30-40mins Curing time 4-6 hours Hardness 20±2 shore A Tear Strength 30N/mm Tensile Strength 3.8Mpa Shrinkage ≤0.3% Elongation 550% ...
... cross-linking at room temperature. The polymerization can be accelerated by heat (max. 1500 C). The silicone components are delivered as liquids, which once mixed and cured transform into a elastic and resi...
...molds making Description of 1:1 liquid platinum silicone rubber for craft molds making MC Silicone MCPLA Addition Cure Series is a two component elastomeric cross-linking at room temperature. The polymerizat...
... elastomeric cross-linking at room temperature. The polymerization can be accelerated by heat (max.1500 C). The silicone components are delivered as liquids, which once mixed and cured transform into a trans...
... elastomeric cross-linking at room temperature. The polymerization can be accelerated by heat (max.1500 C). The silicone components are delivered as liquids, which once mixed and cured transform into a trans...
... Addition Cure Series is a two component elastomeric cross-linking at room temperature. The polymerization can be accelerated by heat (max.1500 C). The silicone components are delivered as liquids, which onc...
...Molds Description of Platinum Silicone Rubber For Mermaid Tail Handicraft Molds MC Silicone MCPLA Addition Cure Series is a two component elastomeric cross-linking at room temperature. The polymerization can...
...Molds Description of Addition Silicone Rubber For Teddy Bear Resin Molds MC Silicone MCPLA Addition Cure Series is a two component elastomeric cross-linking at room temperature. The polymerization can be acc...
... at room temperature. The polymerization can be accelerated by heat (max.1500 C). The silicone components are delivered as liquids, which once mixed and cured transform into a transparent, elastic and resist...
... at room temperature. The polymerization can be accelerated by heat (max.1500 C). The silicone components are delivered as liquids, which once mixed and cured transform into a transparent, elastic and resist...
...Mold Description of Platinum Silicone Rubber For Christmas Tree Silicone Mold MC Silicone MCPLA Addition Cure Series is a two component elastomeric cross-linking at room temperature. The polymerization can b...
...Mold Description of Platinum Silicone Rubber For Halloween Silicone Mold MC Silicone MCPLA Addition Cure Series is a two component elastomeric cross-linking at room temperature. The polymerization can be acc...
...Mold Description of Platinum Silicone Rubber For Rose Candle Silicone Mold MC Silicone MCPLA Addition Cure Series is a two component elastomeric cross-linking at room temperature. The polymerization can be a...
...Molds Description of 10 Shore A Platinum Silicone Rubber For Rabbit Cake Molds MC Silicone MCPLA Addition Cure Series is a two component elastomeric cross-linking at room temperature. The polymerization can ...
...silicone rubber is a two-part, platinum-catalyzed, liquid silicone system that cures (RTV) to a Shore A 0~55 rubber. The polymerization can be accelerated by heat. The silicone components are delivered as li...
... silicone rubber is a two-part, platinum-catalyzed, liquid silicone system that cures (RTV) to a Shore A 0~55 rubber. The polymerization can be accelerated by heat. The silicone components are delivered as l...
... is a two-part, platinum-catalyzed, liquid silicone system that cures (RTV) to a Shore A 0~55 rubber. The polymerization can be accelerated by heat. The silicone components are delivered as liquids,which onc...
... elastomeric cross-linking at room temperature. The polymerization can be accelerated by heat (max.1500 C). The silicone components are delivered as liquids, which once mixed and cured transform into a trans...
... elastomeric cross-linking at room temperature. The polymerization can be accelerated by heat (max.1500 C). The silicone components are delivered as liquids, which once mixed and cured transform into a trans...